An active learning framework for the rapid assessment of galvanic corrosion
Engineering and Technologynpj Materials Degradation

An active learning framework for the rapid assessment of galvanic corrosion

A. Venkatraman, R. M. Katona, et al.

Discover an innovative active learning framework developed by Aditya Venkatraman and colleagues at Sandia National Laboratories. This groundbreaking approach optimizes predictions of galvanic corrosion while significantly reducing computational costs. Understand how low-cost surrogate models can help identify optimal environmental and geometric parameters for improved accuracy in cathodic current predictions.... show more
Abstract
The current present in a galvanic couple can define its resistance or susceptibility to corrosion. However, as the current is dependent upon environmental, material, and geometrical parameters it is experimentally costly to measure. To reduce these costs, Finite Element (FE) simulations can be used to assess the cathodic current but also require experimental inputs to define boundary conditions. Due to these challenges, it is crucial to accelerate predictions and accurately predict the current output for different environments and geometries representative of in-service conditions. Machine learned surrogate models provides a means to accelerate corrosion predictions. However, a one-time cost is incurred in procuring the simulation and experimental dataset necessary to calibrate the surrogate model. Therefore, an active learning protocol is developed through calibration of a low-cost surrogate model for the cathodic current of an exemplar galvanic couple (AA7075-SS304) as a function of environmental and geometric parameters. The surrogate model is calibrated on a dataset of FE simulations, and calculates an acquisition function that identifies specific additional inputs with the maximum potential to improve the current predictions. This is accomplished through a staggered workflow that not only improves and refines prediction, but identifies the points at which the most information is gained, thus enabling expansion to a larger parameter space. The protocols developed and demonstrated in this work provide a powerful tool for screening various forms of corrosion under in-service conditions.
Publisher
npj Materials Degradation
Published On
May 21, 2024
Authors
Aditya Venkatraman, Ryan Michael Katona, Demitri Maestas, Matthew Roop, Philip Noell, David Montes de Oca Zapiain
Tags
active learninggalvanic corrosionsurrogate modelGaussian ProcessNeural NetworkFinite Element simulationscathodic current
Listen, Learn & Level Up
Over 10,000 hours of research content in 25+ fields, available in 22+ languages.
No more digging through PDFs, just hit play and absorb the world's latest research in your language, on your time.
listen to research audio papers with researchbunny